Products Description
ASTM A333 Grade 6 is a seamless carbon steel pipe specifically engineered for low-temperature service where notch toughness is a critical design requirement. It is the most widely specified grade within the ASTM A333/A333M standard, offering the most economical solution for piping systems operating down to −46 °C (−50 °F). Every heat of Grade 6 pipe must pass mandatory Charpy V-notch impact testing at −46 °C, guaranteeing brittle-fracture resistance in cryogenic, cold-climate, and rapid gas-expansion applications.
The pipe is manufactured as a fully killed, fine-grain steel with tighter phosphorus and sulfur limits than standard A106 Grade B, which directly enhances low-temperature toughness. Seamless construction eliminates weld seams as potential crack-initiation sites, making it the preferred form for critical low-temperature piping.
1. Dimensional Range:
| Parameter | Range |
| Nominal Pipe Size (NPS) | 1/8″ – 42″ (DN6 – DN1050); common stock 1/2″ – 36″ |
| Outside Diameter (OD) | 10.3 mm – 1066.8 mm (depends on NPS) |
| Wall Thickness (WT) | 2.0 mm – 14 mm standard; up to 60 mm on request |
| Schedules | SCH 10, 20, 30, STD, 40, 60, XS, 80, 100, 120, 140, 160, XXS |
| Length | Single random (5–7 m), double random (11–13 m), or fixed length up to 18 m / 16,000 mm |
| End Finish | Plain end (square cut) or beveled end 30° +5°/−0° with 1/16″ root face |
Standard reference: ASME B36.10 for wall thickness dimensional correlation.
2. Chemical Composition (ASTM A333 Grade 6, % by mass)
| Element | Requirement |
| Carbon (C), max | 0.3 |
| Manganese (Mn) | 0.29 – 1.06 |
| Phosphorus (P), max | 0.025 |
| Sulfur (S), max | 0.025 |
| Silicon (Si), min | 0.1 |
| Copper (Cu), max | 0.4 |
| Nickel (Ni), max | 0.4 |
| Chromium (Cr), max | 0.3 |
| Molybdenum (Mo), max | 0.12 |
| Vanadium (V), max | 0.08 |
The carbon-manganese balance is intentionally controlled for fine-grain structure and uniform carbide dispersion. Carbon reduction below 0.30% permits a manganese increase above 1.06%, up to a maximum of 1.35%.
3. Mechanical Properties
| Property | Requirement |
| Yield Strength, min | 240 MPa (35 ksi) |
| Tensile Strength, min | 415 MPa (60 ksi) |
| Elongation, min (2″ / 50 mm) | 30% |
| Hardness, max (typical) | 197 HBW |
| Grain Size | Fine grain, ASTM 5 or finer |
Mechanical values are identical to ASTM A106 Grade B in strength, but the defining differentiation lies in the mandatory impact toughness requirement.
4. Mandatory Impact Testing - The Defining Requirement
| Parameter | Requirement |
| Test Temperature | −46 °C (−50 °F) |
| Specimen Orientation | Longitudinal |
| Specimen Size | Full-size 10 × 10 mm when wall thickness permits |
| Minimum Average (3 specimens) | 18 J (13 ft·lbf) |
| Minimum Single Specimen | 14 J (10 ft·lbf) |
| Sub-size Specimens | Proportionally reduced absorbed-energy values per ASTM A333 |
5. Dimensional Tolerances
| OD Range | WT/OD Ratio | Wall Thickness Tolerance |
| 1/8″ ≤ OD ≤ 2 1/2″ | - | +20%/−12.5% |
| 3″ ≤ OD ≤ 18″ | WT/OD ≤ 5% | +22.5%/−12.5% |
| 3″ ≤ OD ≤ 18″ | WT/OD > 5% | +15%/−12.5% |
| OD ≥ 20″ | WT/OD ≤ 5% | +22.5%/−12.5% |
Minimum wall thickness at any point shall not be more than 12.5% under nominal; maximum wall thickness shall not be greater than 20.0% over nominal. For cold-drawn product, tighter tolerances of ±0.1 mm (cold-drawn) or ±0.05 mm (cold-rolled) are achievable on request.
6. Heat Treatment & Manufacturing
Seamless Grade 6 pipe is furnished in the normalized condition (or normalized and tempered). Cold-drawn pipe must be heat-treated after the final cold-draw pass at a temperature not less than 1,500 °F (815 °C) to restore the fine-grain structure and low-temperature toughness. The seamless process involves piercing, rolling, and sizing from a solid billet - no longitudinal weld seam exists, eliminating weld-line toughness degradation.
7. Testing & Inspection (Standard Scope)
- Chemical composition verification
- Tensile test (yield, tensile, elongation)
- Charpy V-notch impact test at −46 °C (mandatory)
- Hydrostatic test (when specified; 2,500 psi for NPS 2 and smaller, held ≥ 5 seconds)
- Nondestructive electric test: eddy current or ultrasonic (standard)
- Surface and dimensional inspection
- Flaring, flattening, bending, hardness tests (as applicable)
8.Packing Methods (Selectable)
| Method | Description | Recommended For |
| Bare packing | Pipes stacked without external wrap; ends protected | Full-container loads, low-risk transit |
| Bundle packing | Uniform-length pipes banded with same-material strips; hexagonal or square bundles available | NPS > 2″ to 6″; general export |
| Crate packing / Wooden case | Pipes enclosed in wooden crates, plastic-wrapped inside | NPS ≤ 2″ and thin-wall (≤ 3.2 mm) to prevent denting; high-value or mixed-size orders |
| Wooden protection at both ends | Timber reinforced at pipe ends within bundles | Sea-worthy delivery where end deformation risk exists |
| Plastic wrapping + oiling | Internal corrosion protection for pickled/oiled or bare surface | Long ocean transit, humid climates |
Bundle weight limit: ≤ 2,000 kg per bundle (typical export standard). Pipe lengths for container loading are commonly limited to 11.8 m.
Loading Options
- Bulk vessel for large-diameter / heavy-wall projects
- Container loading (20′ / 40′) for NPS ≤ 16″ and lengths ≤ 11.8 m
- Breakbulk for lengths exceeding container limits


Application Areas
ASTM A333 Grade 6 is selected wherever carbon steel piping is exposed to temperatures at or below −29 °C, the threshold below which ASME B31.3 typically requires impact-tested material. Its cost-to-performance balance makes it the default low-temperature carbon steel grade for:
| Industry / Application | Typical Service |
| Oil & Gas Processing | Low-temperature process lines, gas processing, depressurization/blowdown systems where rapid gas expansion causes severe cooling |
| LNG & Cryogenic Terminals | LNG transport lines, cold boxes, liquefaction units operating at −46 °C and above (for lower temperatures, Grade 3 or Grade 8 is required) |
| Petrochemical & Refining | Low-temperature fractionation, refrigeration loops, and process piping in cold-service trains |
| LPG / Propane Storage & Handling | Service temperatures down to approximately −42 °C |
| Cold-Climate Pipelines | Pipeline stations, block valve stations, and above-ground piping in Arctic and sub-Arctic environments |
| Air Cooler Outlet Piping | Cold ambient conditions where the pipe wall sees sub-zero metal temperatures during operation or shutdown |
| Power Generation & Marine | Low-temperature auxiliary piping, shipbuilding, and offshore modules in cold-service zones |
Grade selection quick rule: Above −29 °C → A106 Gr. B. −29 °C to −46 °C → A333 Gr. 6. −46 °C to −101 °C → A333 Gr. 3. Below −101 °C → A333 Gr. 8 or austenitic stainless.
FAQ
Q1: What is the difference between ASTM A333 Grade 6 and Grade 3?
The primary difference is the minimum impact test temperature. Grade 6 is tested at −46 °C (−50 °F); Grade 3 is tested at −101 °C (−150 °F) and contains approximately 3.5% nickel to achieve the lower ductile-to-brittle transition temperature. Grade 6 is nickel-free (Ni ≤ 0.40%) and is the more economical choice for service temperatures down to −46 °C. Below that threshold, Grade 3 or Grade 8 is required.
Q2: Can A333 Grade 6 be substituted for A106 Grade B?
No, not for low-temperature service. The two grades share similar tensile and yield strengths, but A106 Grade B has no mandatory Charpy impact testing requirement. ASME B31.3 generally limits A106 Gr. B to −29 °C without impact testing. A333 Gr. 6 is the correct specification whenever the design metal temperature falls below that threshold. Conversely, A333 Gr. 6 is not intended for elevated-temperature service above approximately 343 °C (650 °F).
Q3: Is impact testing always required for A333 Grade 6?
Yes. Charpy V-notch impact testing at −46 °C is a mandatory acceptance test for every heat/lot of Grade 6 pipe. It is not a supplementary requirement that must be separately invoked. The minimum average absorbed energy for three full-size specimens is 18 J (13 ft·lbf), with no single specimen below 14 J (10 ft·lbf).
Q4: What heat treatment is required?
Seamless A333 Grade 6 is furnished in the normalized condition. If the pipe is cold-drawn, it must be heat-treated after the final cold-draw pass at ≥ 1,500 °F (815 °C) to restore the fine-grain structure necessary for low-temperature toughness. The standard requires the pipe to be fully killed and fine-grain treated (ASTM grain size 5 or finer).
Q5: What matching fittings and flanges should be used with A333 Gr. 6 pipe?
Low-temperature-rated components must be specified throughout the system. The standard matching items are:
Fittings: ASTM A420 WPL6 (instead of A234 WPB)
Flanges / forgings: ASTM A350 LF2 (instead of A105)
Using ambient-temperature-rated components in a low-temperature system reintroduces brittle-fracture risk at the connection points.
Q6: Can A333 Gr. 6 pipe be supplied with a lower impact test temperature than −46 °C?
Yes, by purchaser specification. If the design metal temperature is lower than the standard test temperature, the purchaser may order impact testing at a lower temperature, and the required absorbed energy is stated explicitly on the order and mill certificate. However, the standard grade designation remains Grade 6; the lower test temperature is a supplementary contractual requirement.
Q7: What is the difference between ASTM A333 and ASME SA333?
The two designations are technically equivalent. ASTM A333/A333M is the base material specification; ASME SA333/SA333M is the ASME Code adoption of the same specification, used for ASME Boiler & Pressure Vessel Code stamped components. Pipe dual-certified to both A333 and SA333 satisfies either procurement route without material property differences.
Our address
Rm1406,14th/F No 208, Hongqi Road, Nankai Dist, Tianjin City ,China
Phone Number( WhatsApp/wechat)
+8616622033809
alisa@tjshenzhoutong.com

Hot Tags: astm a333 grade 6 seamless steel pipe tube sch40 sch80 sch160, China astm a333 grade 6 seamless steel pipe tube sch40 sch80 sch160 manufacturers, suppliers, factory, seamless pipe for cap connection, seamless pipe for marking system connection, seamless pipe for mitigated operation in industry, seamless pipe for mitigated operation system connection, seamless pipe for recovery system connection, seamless pipe for testing system connection